Paper and Plastic Fresh Tray Selection Limits by Category
A customer of ours moved a chilled diced beef line from PP to a fibre tray. Sustainability commitment. It looked fine for two days. On the third, the base corners went soft, the lidding film lifted at one corner without tearing, and the batch came off shelf. Nothing was wrong with the meat. What killed the tray was roughly two tablespoons of purge sitting in the bottom since packing.
Nobody asked where the format would break. In tray selection that's the only question worth asking and it mostly doesn't get asked. People ask which material is better, which is greener, which is cheaper per unit. None of those can be answered before you know what the product does to the tray over its shelf life.

It isn't a material property
Six things decide whether a tray survives, and a product can break a format on any one of them. Free liquid, meaning purge, brine or meltwater, and how many days it sits there. Fat and acid, which go after coatings in a way water doesn't. The real temperature window, cold store to shelf included, not just the rating on the spec sheet. Load, which is how far the base deflects once a full stack has stood for an hour. Whether it seals on your machine at all, and holds a modified atmosphere if you need one. And what your waste contractor actually accepts, which is not the same question as what the tray is made of.
Whichever of those gives way first is the limit. The rest is marketing.
Raw meat, poultry, fish
Hardest group for paper. Purge collects, the base stays wet, fibre loses stiffness from the bottom up. Wet strength additives delay that, they don't prevent it. Once the base deflects the walls bow and the rim distorts, and a distorted rim lets the film go without tearing it, so it reads as a sealing fault when it's structural. Fish is worse than beef because of standing meltwater.
For red meat the decisive one is gas. High oxygen MAP holds the bloom and fibre can't hold MAP without a barrier layer. So the crossover is a spec, not a feeling: the moment shelf life or presentation needs MAP, plain fibre is out.
Watch the displaced cost too. Most fibre trays on a fresh counter are paper plus a PE or PP layer, and the performance comes from the layer. Your recycling claim now depends on a composite the receiving facility may not separate. A supplier who won't state coat weight isn't giving you a spec.
Produce, and where visibility counts
Produce breaks differently. Here the enemy is water in the air. Mushrooms, berries and whole fruit do better in something that doesn't trap moisture, and breathable fibre handles it. Plastic needs perforation or anti-fog, otherwise you get spoilage under a misted lid. Cut fruit and salad run the other way, and not for material reasons. Visibility is a real category requirement.

Heat, fat, freeze cycles
PP goes to roughly 120–130 °C. Fine for microwave, nowhere near an oven, which is where coated fibre wins. Something baked in the tray, chilled, then microwaved in store is asking for two windows at once. In practice that means changing format between production and retail rather than hunting for a cleverer tray.
Frozen fails on cycles, not temperature. An unlaminated fibre tray can delaminate after two thaw and refreeze rounds. Ask how many times the product crosses the freeze line before you ask for a price.
One shift is enough to test it
Fill to real net weight and leave it a day. Measure base deflection, photograph the rim at one, four and twenty-four hours. Tilt the heaviest tray to the steepest angle on your actual route and hold it fifteen seconds. Walk the cold store to shelf transition and see where condensation lands. Peel the film: if it comes away clean with no fibre or coating, it was never bonded. Soak a composite edge overnight and check whether the layers separate.
None of this picks a material for you. But if you're retraining operators to fix what looks like a sealing problem, you probably have a format limit you haven't measured.